From: The effect of Er, Cr:YSGG laser debonding on the bond strength of two ceramic materials to dentin
Shear bond strength (mean ± SD) | p-value | |||
---|---|---|---|---|
Lithium disilicate -Bond | Lithium disilicate -Rebond | Ultra-translucent zirconia-Bond | Ultra-translucent zirconia-Rebond | |
6.53 ± 1.60a | 1.12 ± 0.05c | 6.43 ± 2.28a | 4.33 ± 1.88b | < 0.001* |