Skip to main content

Table 1 Surface modifications and fixture resin used for different test groups

From: In vitro evaluation of the influence of titanium nitride coating on the retention force between components of two-part abutments

Group

Titanium bases (n = 30)

Zirconia build-ups (n = 30)

Luting Agent

Mechanical

Chemical

Mechanical

Chemical

A (n = 10)

110 µm Al2O3

 

110 µm Al2O3

 

Panavia F 2.0

B (n = 10)

110 µm Al2O3

Alloy Primer

110 µm Al2O3

Clearfil Ceramic Primer

Panavia F 2.0

C (n = 10)

110 µm Al2O3

Clearfil Ceramic Primer

110 µm Al2O3

Clearfil Ceramic Primer

Panavia F 2.0

Group

Titanium nitride coated bases (n = 30)

Zirconia build-ups (n = 30)

Luting agent

Mechanical

Chemical

Mechanical

Chemical

D (n = 10)

110 µm Al2O3 before coating

 

110 µm Al2O3

 

Panavia F 2.0

E (n = 10)

110 µm Al2O3 before coating

Alloy Primer

110 µm Al2O3

Clearfil Ceramic Primer

Panavia F 2.0

F (n = 10)

110 µm Al2O3 before coating

Clearfil Ceramic Primer

110 µm Al2O3

Clearfil Ceramic Primer

Panavia F 2.0